Polymer Property : Core Loss = 0.00324 W/kg Product List

Magnetic Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Magnetic Properties Metric English Comments
Core Loss 0.00324 W/kg

@Magnetic Field 0.100 T,
Frequency 50.0 Hz
0.00147 W/lb

@Magnetic Field 0.100 T,
Frequency 50.0 Hz
Sheet, 0.009"; ASTM A804
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..