Polymer Property : K Factor (ISO) = 6.0 µm/km Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP Fluorosint® MT-01 PTFE + additives, enhanced grade, compression moulded (ISO Data)
Fluorosint MT-01 is an extreme service grade developed specifically for applications where the benefits of PTFE-based materials also require strength, stiffness and stability. Fluorosint MT-01 deliv..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data)
Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data)
TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data)
Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data)
TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data)
TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data)
This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne..
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data)
TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid..