Mechanical Properties Metric English Comments
K Factor (ISO) 70 µm/km
70 µm/km
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data)
This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi..