Tensile Impact | 534 J/cm | 1000 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 1584 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 534 J/cm | 1000 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 1938 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 534 J/cm | 1000 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7597 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |