Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 55.5 J/cm | 104 ft-lb/in | Warp |
Hexcel® HexForce™ 383 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 55.5 J/cm | 104 ft-lb/in | Filling |
Hexcel® HexForce™ 383 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |