Polymer Property : Tensile Impact = 110 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 58.7 J/cm
110 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 1614 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 58.7 J/cm
110 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 6080 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 58.7 J/cm
110 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 1579 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..