Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 120 J/cm | 225 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 1526 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 120 J/cm | 225 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7626 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |