Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 726 J/cm | 1360 ft-lb/in | Warp |
Hexcel® HexForce™ 384 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |