Mechanical Properties Metric English Comments
Tensile Impact 86.0 J/cm
161 ft-lb/in
ASTM D1822
LyondellBasell Alathon® L5440 High Density Polyethylene
ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch..