Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 246 J/cm | 460 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1800 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 246 J/cm | 460 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7581 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 246 J/cm | 460 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 7581 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |