Polymer Property : Tensile Impact = 6.67 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 6.67 J/cm
12.5 ft-lb/in
Force Deflection at 30%; ASTM D575 Modified
Parker Chomerics CHOFORM® 5560 Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..