Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 481 J/cm | 900 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1584 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 481 J/cm | 900 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1938 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |