Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 2.40 N | 0.540 lb (f) | MD; ISO 6383/2 |
Borealis Himod™ FT3280 LDPE for Film Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Tear Strength, Total | 2.40 N | 0.540 lb (f) | M.D., Elmendorf; ASTM D1922 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |