Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 14.0 N | 3.15 lb (f) | Initial in TD; ASTM D1004 |
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |