Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 2140 N | 481 lb (f) | Graves, MD; ASTM D1004 |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |