Mechanical Properties Metric English Comments
Tear Strength, Total 16.0 N
3.60 lb (f)
Split Tear Method, 254mm/min, TD; ASTM D1938
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Tear Strength, Total 16.0 N
3.60 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Tear Strength, Total 16.0 N
3.60 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Tear Strength, Total 16.0 N
3.60 lb (f)
Split Tear Method, 254mm/min, TD; ASTM D1938
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..