Tear Strength, Total 370 N
83.2 lb (f)
ASTM D1004
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Tear Strength, Total 370 N
83.2 lb (f)
ASTM D1004
Eastman Neostar FN005 Elastomer
Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough..