Mechanical Properties Metric English Comments
Tear Strength, Total 8.00 N
1.80 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Tear Strength, Total 8.00 N
1.80 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Tear Strength, Total 8.00 N
1.80 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Tear Strength, Total 8.00 N
1.80 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness
Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: ..
Tear Strength, Total 8.00 N
1.80 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..