Mechanical Properties Metric English Comments
Tear Strength, Total 42.0 N
9.44 lb (f)
90° Tear Resistance, MD; ASTM D1004
Eastman Sahara Film
Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films
Tear Strength, Total 42.0 N
9.44 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Tear Strength, Total 42.0 N
9.44 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..