Polymer Property : Tensile Strength = 0.230 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 0.230 MPa
33.4 psi
ISO 7214 1998
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam
Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi..