Mechanical Properties Metric English Comments
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9035 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9225 K 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9335 MG 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Tensile Strength 0.880 MPa
128 psi
DIN EN ISO 1798
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..