Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.90 - 7.00 MPa | 421 - 1020 psi | ASTM D 638 |
API Megol AM DP1741 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tensile Strength | 3.50 - 7.00 MPa | 508 - 1020 psi | ASTM D 638 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |