Mechanical Properties Metric English Comments
Tensile Strength 7.081 MPa
1027 psi
Silicone Property; ASTM D412
Arlon LW3015B##-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.5 inch wide, 30 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll leng..