Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.467 MPa | 1083 psi | Silicone Property; ASTM D412 |
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Tensile Strength | 7.467 MPa | 1083 psi | Silicone Property; ASTM D412 |
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |