Polymer Property : Tensile Strength = 11.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Addisilâ„¢ 1050 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Addisilâ„¢ 2050 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Addisilâ„¢ 440 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Silplusâ„¢ 70 HS High Strength Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
IEC 60811-1-1
Lucobit Lucofin® 7440 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Addisilâ„¢ 442 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Addisilâ„¢ 450 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
Momentive Performance Materials Addisilâ„¢ 452 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 11.5 MPa
1670 psi
ASTM D412
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD ..
Tensile Strength 11.5 MPa
1670 psi
ISO 527
Fainplast Compounds Hax™ HF 215 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flame retardancy, improved processabilityInformation provided by Fainplast Compound..
Tensile Strength 11.5 MPa
1670 psi
300; ISO 37
BASF Elastollan SP 806 TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 11.5 MPa
1670 psi
AlphaGary Megolon™ HF 8110 Low Smoke Halogen Free
General purpose sheathing compound with good mechanical and processing properties. Application examples include Data Cables, Optical Cables.
Tensile Strength 11.5 MPa
1670 psi
AlphaGary Megolon™ S540E Low Smoke Halogen Free
Highly flexible sheathing grade with a low Young's Modulus and excellent fire retardancy, offering improved processability. Application examples include Radio Frequency / Data Optical / Special Fire..
Tensile Strength 11.5 MPa
1670 psi
ISO 37
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer
Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding..
Tensile Strength 11.5 MPa
1670 psi
AlphaGary Megolon™ S530 Low Smoke Halogen Free
Highly flexible sheathing grade with a low Young's Modulus and excellent fire retardancy. Application example includes Radio Frequency.
Tensile Strength 11.5 MPa
1670 psi
ISO 527
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound..