Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 655 - 793 MPa | 95000 - 115000 psi | Annealed Bar |
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan.. |