Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 1170 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 1170 MPa

@Temperature 400 °C
170000 psi

@Temperature 752 °F
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel
Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica..