Mechanical Properties Metric English Comments
Tensile Strength 119 MPa

@Temperature 150 °C
17300 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8549 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance..