Polymer Property : Tensile Strength = 12.232 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 12.232 MPa

@Temperature 60.0 °C,
Time 605000 sec
1774.1 psi

@Temperature 140 °F,
Time 168 hour
Oil Aged
S&E Specialty Polymers TufTech™ GA-509OR-JM PVC Compound
Application: An 80°C, oil resistant, flexible PVC based compound suitable for jacketing applications.Information provided by S&E Specialty Polymers