Polymer Property : Tensile Strength = 12.51 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 12.51 MPa
1815 psi
Cyclewood Solutions Xylomer™ XM1-KJD Injection Molding Compostable Resin
100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an ab..