Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 12.53 MPa | 1818 psi | ASTM D412 |
Northstar Polymers MPP-A80H Room-Temperature Curable Polyurethane MPP-A80H has been specifically formulated to service applications where high elongation and good physical strength are required as well as where temperature during the process must be low for a very.. |