Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 12.896 MPa @Time 605000 sec |
1870.4 psi @Time 168 hour |
Aged in ASTM Oil #2 |
S&E Specialty Polymers TufFlex™ GA-1042FR-60-0-405 Black TPE Compound Application: An oil resistant, flexible, 60°C rated jacketing compound.Information provided by S&E Specialty Polymers |