Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 830 MPa | 120000 psi | |
H.C. Starck HPM 1800 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength | 830 MPa | 120000 psi | |
H.C. Starck HPM 1810 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength | 830 MPa | 120000 psi | |
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |