Polymer Property : Tensile Strength = 1217 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.391 MPa
1217 psi
Silicone Property; Arlon SQA-TMS-009
Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape
1 inch wide, 30 mil thick, 12.0 yards long, red, triangular cross-section, self-fusing silicone tape.Design/Construction:Interleave: 1 mil PETProduct: Cured Silicone Self-fusing RubberCross-section..