Mechanical Properties Metric English Comments
Tensile Strength 122.6 MPa
17790 psi
ASTM D638
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
Tensile Strength 122.6 MPa
17790 psi
ASTM D638
E-Polymers SEPAZ® N5020HI Nanoclay 4%, 30% Glass Fiber Reinforced High Impact Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Tensile Strength 122.6 MPa
17790 psi
ASTM D638
E-Polymers TEKAMID® JN920 PPE+PA66 20% Glass Fiber Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..