Tensile Strength 87.309 MPa
12663 psi
ASTM D638
E-Polymers TEKAPPO® J920 20% Glass Fiber Reinforced M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..