Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 88.0 MPa | 12800 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Tensile Strength | 88.0 MPa | 12800 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Tensile Strength | 88.0 MPa | 12800 psi | ASTM D638 |
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon. |
|||
Tensile Strength | 88.0 MPa | 12800 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Tensile Strength | 88.3 MPa | 12800 psi | ASTM D638 |
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (.. |
|||
Tensile Strength | 88.3 MPa | 12800 psi | ASTM D638 |
Samyang Tribit® 1551GN15 PBT, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN15 is a reinforced, flame retardant g.. |
|||
Tensile Strength | 88.3 MPa | 12800 psi | ASTM D638 |
Samyang Trirex® 3025GNH15 Polycarbonate, Reinforced Flame Retardancy, Non-Halogen PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GNH15 is a reinforced, flame retardant, non-halogen grade.Applications: LCD Panel .. |
|||
Tensile Strength | 88.0 MPa @Temperature 23.0 °C |
12800 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT™ 2021 Polyimide, Brown (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Tensile Strength | 88.0 MPa @Strain 10.0 %, Temperature 0.000 °C |
12800 psi @Strain 10.0 %, Temperature 32.0 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 88.3 MPa | 12800 psi | ASTM D638 |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Tensile Strength | 88.0 MPa | 12800 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |