Polymer Property : Tensile Strength = 12880 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 88.78 MPa
12880 psi
ASTM D638
E-Polymers SEPAZ® N4040M1 Dimensional Stability Heat Resistance Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..