Mechanical Properties Metric English Comments
Tensile Strength 0.895 MPa
130 psi
ISO 7214 1998
Zotefoams Evazote® VA80 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..