Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 130000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 896 - 979 MPa
130000 - 142000 psi
International Mold Steel TOOLOX 33 Cold Work Die Steel
TOOLOX 33 is a quenched and tempered tool steel designed to have low residual stresses and extremely good machinability. Applications include: Plastic molds; Rubber molds; Bending tools; Machine com..