Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 94.0 MPa @Temperature 23.0 °C |
13600 psi @Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® RE5231 BK533 PET
(Unverified Data**) Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 94.0 MPa | 13600 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Tensile Strength | 93.8 MPa | 13600 psi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Tensile Strength | 94.0 MPa | 13600 psi | ASTM D638 |
Kolon KOCETAL® GF302 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties.Information provided by API-Kolon. |
|||
Tensile Strength | 94.0 MPa | 13600 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Tensile Strength | 93.8 MPa | 13600 psi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |