Polymer Property : Tensile Strength = 13659 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 94.176 MPa
13659 psi
ASTM D638
E-Polymers TEKAMID® JN910 PPE+PA66 10% Glass Fiber Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..