Polymer Property : Tensile Strength = 1550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 10.7 MPa

@Treatment Temp. 121 °C,
Time 605000 sec
>= 1550 psi

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged
S&E Specialty Polymers GTPO 9100HF Series PVC
Application: New generation 80/90C, UV Resistant, low gravity, flexible, polyolefin based Zero Halogen compound with good physical characteristics.Information provided by S&E Specialty Pol..
Tensile Strength 10.7 MPa
1550 psi
Optimum; With provided formulation; ASTM D638
PolyOne Geon™ 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Adept E49 is a low molecular weight homopolymer dispersion resins intended for use in variety of plastisol applications and processes. It reduces scrap rates and manufacturing costs by extend..
Tensile Strength 10.7 MPa

@Strain 100 %
1550 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 10.7 MPa

@Strain 100 %
1550 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 86155 Polyvinyl Chloride, Flexible (PVC, Flexible)
86155 is a flexible (90A durometer) vinyl compound formulated from FDA-santioned raw materials. This compound has received NSF Standard 61 only for sheets applications.NOTE: All ingredients used in ..
Tensile Strength 10.7 MPa
1550 psi
Aged 7 days @ 110°C; IEC 60811-1-1
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Tensile Strength 10.7 MPa
1550 psi
Teknor Apex Elexar® EL-8730A Thermoplastic Elastomer
Notes: Sunlight Resistant; Temperature Rating: 125°C Processing Method: Extrusion; Injection MoldingInformation Provided by Teknor Apex