Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 157 MPa | 22800 psi | ASTM D638 |
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66 EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon. |
|||
Tensile Strength | 157 MPa | 22800 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BBG30-AN00N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 157 MPa | 22800 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |