Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 16.7 MPa | >= 2420 psi | ASTM D 638 |
Karina 750D10/120-IS-PO White PVC Compound PVC powder compound, recommended for covering metallic parts in fluidized bed.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 16.7 MPa | 2420 psi | |
Teknor Apex Elexar® EL-8451 Thermoplastic Elastomer Notes: Sunlight Resistant; Temperature Rating: 105°C Processing Method: Extrusion; Injection MoldingInformation Provided by Teknor Apex |