Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.12 MPa | 162 psi | ISO 7214 1998 |
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |