Polymer Property : Tensile Strength = 168.2 MPa
Polymer Property :
Tensile Strength =
168.2 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength
168.2
MPa
24390
psi
50 mm/min; ISO 527-1,-2
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.