Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 12.5 MPa | >= 1810 psi | Type IV, 500mm/min; ASTM D638 |
S&E Specialty Polymers XP23-45MG PVC Description: PVC weatherable, integral colored, filledApplication: Body side molding end caps and extruded skin compound which meets Chrysler MSDC 543 and Ford WSK-M4D689-A3Information provided by .. |
|||
Tensile Strength | 12.5 MPa | 1810 psi | |
Momentive Performance Materials Silplusâ„¢ 60 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 12.5 MPa | 1810 psi | Crosslinked specimen; ISO 527 |
Fainplast Compounds Hax™ HFX 507 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; Insulation; easy processingInformation provided.. |
|||
Tensile Strength | 12.5 MPa | 1810 psi | Crosslinked specimen; ISO 527 |
Fainplast Compounds Hax™ HFX 509/1 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Tensile Strength | 12.5 MPa | 1810 psi | ISO 527 |
Fainplast Compounds Hax™ HF 045/16M Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Tensile Strength | 12.5 MPa | 1810 psi | ISO 527 |
Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds |
|||
Tensile Strength | 12.5 MPa | 1810 psi | |
AlphaGary Megolon™ S642 Low Smoke Halogen Free A thermoplastic, halogen free, fire retardant, low smoke and fume cable compound. This sheathing grade exhibits an excellent level of fire retardancy and has been developed to meet the requirements .. |