Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 184.4 MPa
26750 psi
ASTM D638
E-Polymers SEPAZ® V330HS 30% Glass Fiber Reinforced Heat Stabilized PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..