Mechanical Properties Metric English Comments
Tensile Strength 130.9 MPa
18990 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 130.9 MPa
18990 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.